Skip to content
Foundry Consumable · Cincin Degassing untuk Peleburan Tembaga, Kuningan & Perunggu

Logas Degassing Rings Supplier in Indonesia

Gas-releasing ring plunged into copper melts · for hydrogen removal and oxide flotation

Chelora Chemicals supplies Logas, a pressed degassing ring for copper and copper-alloy melts, to brass, bronze and copper foundries across Indonesia. In Bahasa Indonesia the product is called cincin degassing tembaga. The ring is plunged below the melt surface on a plunger rod, where it releases gas that flushes dissolved hydrogen out of the metal and helps carry oxide particles to the surface, reducing gas porosity in castings. Logas is a copper-alloy product and is not used for aluminium; for aluminium melts see Degasar. Rings are supplied in moisture-protected packs, with ring weight and moisture shown on every certificate of analysis.

CoA with every batchGHS SDS · transport documentsFOB · CFR · CIF · DAPPengiriman ke seluruh Indonesia
Identification Sheet Foundry Consumable
ProductLogas degassing ring
Product typePressed gas-releasing ring
Used inCopper, brass and bronze melts
FunctionHydrogen removal, oxide flotation
FormPressed rings with centre hole
Ring weightAgreed per order
CompositionFormulation-specific; stated in batch SDS
Moisture0.5% max (indicative)
HS code3810.90 or 3824.99 (broker to confirm)
Transport classPer batch SDS
PackingMoisture-barrier packs in cartons
SynonymsDegassing ring, purging ring, cincin degassing tembaga
Primary DutyDegassinghydrogen removal from copper melts
FormPressed ringcentre hole for plunger rod
AlloysCopper alloysbrass, bronze, copper
Key Quality PointDrynessmoisture is the first CoA value to read
Not ForAluminiumuse a tablet made for aluminium
Grades OfferedStandard / Premiumtighter limits on premium
01 / PRODUCT DOSSIER

What Logas is: a degassing ring for cleaner copper-alloy castings

What the ring does in the melt, how it differs from deoxidising tubes and slag coagulants, why foundries use it, and how Chelora Chemicals supplies it to Indonesian buyers.

Molten copper alloys pick up hydrogen from moisture in the charge, fuel gases and tools, and the gas is released again on freezing, leaving pinholes and porosity in the casting. Logas is a pressed ring made to treat the melt before pouring. It is held on a plunger rod, pushed to the bottom of the crucible or ladle and left to react, and the gas it releases rises through the metal as bubbles that carry hydrogen away and float out some oxide particles.

Hydrogen is only one of the gases a copper melt carries. Dissolved oxygen is removed separately with Deoxidising Tubes, and surface slag is handled with a coagulant such as Slax 30. A typical copper-alloy melt shop uses these steps in sequence rather than expecting one product to do every job.

Why foundries use it

A ring needs no gas lines or rotor and works with the crucibles and ladles a brass or bronze foundry already has. It is widely used where castings must be pressure-tight, such as valves, pump parts, fittings and bearings.

Logas versus deoxidising tubes and fluxes

Logas removes dissolved hydrogen. Deoxidising Tubes remove dissolved oxygen, and a slag coagulant like Slax 30 separates slag from the metal. The aluminium equivalent of a degassing ring is a tablet such as Degasar, which is made for a different melt chemistry.

Choosing for the alloy

Not every copper alloy is degassed the same way. Aluminium bronzes and other alloys with reactive elements may need different treatment, so we confirm the product against your alloy before quoting.

A supplier, not a manufacturer

Chelora Chemicals buys Logas from vetted manufacturing partners, agrees the specification with you before the purchase order, checks each batch’s documents against it, and manages packing, paperwork and freight to your port or plant. We give no process doses.

02 / PHYSICAL & CHEMICAL PROPERTIES

Logas properties: ring form, dryness and gas release

Typical values for a commercial copper-alloy degassing ring, for orientation. The figures for your shipment are confirmed on the certificate of analysis and the SDS for that batch.

Physical PropertyTypical Value
Physical formPressed ring with centre hole
ColourOff-white to grey, formulation dependent
Ring weightAgreed per order
Outer diameterMatched to the plunger rod and crucible, agreed per order
HardnessFirm, non-dusting when intact
Moisture0.5% max, indicative
Gas releaseStarts on contact with molten metal
Solubility in waterFormulation dependent; treat as water-sensitive
Handling / Safety PropertyTypical Value
Water contactMoisture weakens the ring and can cause spitting; keep sealed
Flash pointNot applicable as a solid
StabilityStable in sealed original packs
Incompatible materialsAcids, water and wet storage
Reactions to noteGas and fume release in the melt; ring must be fully submerged
Fume on useMetal-oxide and salt fume; extraction needed over the furnace
ResidueSmall amount of dross or salt floats to the surface
Typical classificationPer batch SDS, depends on formulation
03 / GRADE SPECIFICATION

Logas specification: ring weight, moisture, composition class and strength

Indicative limits for the two grades we quote. The binding specification is the one in your quotation and is confirmed on each certificate of analysis.

ParameterTest MethodStandard GradePremium Grade
AppearanceVisualPressed rings, uniform colourPressed rings, uniform colour, no cracks
Ring weightBalance, 20 rings± 5% of nominal± 3% of nominal
Outer / inner diameterVernier caliperAgreed per order, ± 1 mmAgreed per order, ± 0.5 mm
MoistureLoss on drying≤ 0.5%≤ 0.3%
Crushing strengthCompression testReportedReported, tighter minimum
Broken or chipped ringsVisual count≤ 2% of lot≤ 1% of lot
Gas releaseLaboratory gas-release testReportedReported
Composition classSDS / formulation statementAs quotedAs quoted
PackingVisualMoisture-barrier packs in cartonsIndividually sealed packs in cartons

Limits are indicative and are not a performance guarantee. Foundries often write their own limits for ring weight, dimensions and dryness. Send us your specification and the test methods it names, and we confirm what our manufacturing partner can guarantee before you order.

04 / MANUFACTURING ROUTE

How degassing rings are made: blending, pressing and sealed packing

An outline of the general route, for orientation. Our manufacturing partners’ formulations and process conditions are proprietary and are shared only as far as needed to read the certificate of analysis.

Degassing rings are made by blending dry powders and pressing them into rings with a centre hole for the plunger rod. The formulation sets the gas volume, the rate of release and the amount of fume, and it is chosen for copper-alloy melt temperatures, which are higher than aluminium melts.

After blending, the powder is pressed, the rings are inspected for weight, dimensions and cracks, and they are packed at once in moisture-barrier bags. Because the ingredients attract water, rings left open before packing lose strength and can spit when they hit the melt.

Quality depends on raw-material dryness, blend uniformity, press settings and pack integrity. That is why moisture, ring weight and breakage are the numbers a foundry should read first on a CoA.

05 / APPLICATIONS

Logas uses in Indonesia: degassing in brass, bronze and copper foundries

Where foundry and metallurgical buyers use copper-alloy degassing rings. Practice varies by alloy, so we ask about your process before quoting.

Field 01

Brass Foundries

Brass casters of valves, fittings and plumbing parts degas melts to reduce porosity that causes leaks under pressure.

Field 02

Bronze & Gunmetal Casting

Casters of bearings, bushes, marine and pump parts treat tin bronze and gunmetal melts before pouring.

Field 03

Copper & Red Brass Casting

Copper-alloy foundries use degassing to keep castings sound, together with deoxidation of the melt.

Field 04

Pump & Valve Components

Pressure-retaining parts need low porosity, so degassing is a routine step before pouring.

Field 05

Sand & Gravity Casting

Sand and gravity foundries use rings in crucibles and transfer ladles where no gas-purging equipment is installed.

Field 06

Ingot & Remelting

Remelters of copper-alloy scrap use degassing to clean the melt before casting ingot.

Field 07

Training & Test Laboratories

Universities and laboratories use rings in melt-treatment demonstrations and porosity studies.

Field 08

Combined Melt Treatment

Logas works with Deoxidising Tubes for oxygen removal and Slax 30 for slag control in a full copper-alloy practice.

06 / REACTION CHEMISTRY

Logas chemistry: hydrogen in copper melts, gas release and flotation

Five behaviours explain almost everything a foundry sees when it uses a degassing ring in copper alloys.

Hydrogen Pickup

Copper melts take up hydrogen from damp charge, fuel combustion products and wet tools. Hydrogen is much less soluble in solid metal, so it is rejected on freezing and forms pores.

Gas Release from the Ring

On contact with the hot melt, the ring decomposes and releases gas. The composition is formulation-specific and stated in the SDS.

Hydrogen Transfer to Bubbles

Hydrogen diffuses from the melt into the rising bubbles because the gas inside has a low hydrogen content, and leaves the melt with them.

Flotation of Oxides

Rising bubbles carry oxide films and fine particles to the surface, where Slax 30 or a similar coagulant helps separate them with the slag.

Oxygen and Hydrogen Together

In copper, dissolved oxygen and hydrogen can combine to form steam and cause porosity, which is why Deoxidising Tubes are used alongside degassing.

07 / RELATED BUILDING BLOCKS

Logas and related foundry products we supply

Buyers compare degassing rings with other melt-treatment products for copper alloys. This table sets out how each relates to Logas.

ProductReferenceRelationship to LogasNotes
LogasFoundry ringThis productPressed degassing ring for copper, brass and bronze melts, in standard and premium grades.
Deoxidising TubesCopper tubesUsed togetherRemove dissolved oxygen from copper-alloy melts.
Slax 30Slag coagulantUsed togetherCoagulates slag so it can be skimmed from the melt.
Degasar (Degassing Tablet)Degassing tabletAluminium counterpartDegassing tablet made for aluminium melts, not copper alloys.
Granulated FluxCleaning fluxRelated melt cleaningGranular cleaning and drossing flux for aluminium melts.

Exact compositions and specifications are confirmed per batch on the certificate of analysis. For products other than Logas, treat the notes above as a sourcing guide, not a specification sheet.

08 / HAZARD & HANDLING

Logas hazards: fume, moisture and molten-metal safety

General guidance for degassing rings. Classification differs between formulations, so always work from the current SDS supplied with your batch.

Classification

Depends on formulation. The SDS for your batch gives hazard statements.

Moisture + Molten Metal

Damp rings, tools or plungers can spit or cause violent steam release in molten copper alloy. Keep everything dry and preheated.

Fume

Treatment releases fume and fine particulate. Extract above the furnace and avoid breathing it.

Dust

Broken rings can produce dust. Handle gently and avoid dry sweeping.

PPE Standard

Face shield, heat-resistant gloves, aluminised apron, safety boots and a suitable respirator as the risk assessment requires.

Reactive Handling

Keep away from acids and wet areas.

Spill & Waste

Collect spilt rings dry. Dispose of dross and salt residue through licensed channels.

Fire

Rings are not a fuel; use the extinguishing media in the SDS.

First Aid: Eyes & Skin

Rinse eyes with water for several minutes; wash skin with soap and water; seek advice if irritation persists.

First Aid: Inhalation

Move to fresh air. Seek medical advice if symptoms continue.

Transport

Shipping class follows the batch SDS, Section 14; some formulations are not regulated, others are.

Signal Word & Pictograms

As stated on the SDS and label for the formulation supplied.

Safety data sheets for degassing rings vary with formulation, which is why the SDS for your batch is the reference. The main practical hazards are moisture in contact with molten metal, fume over the furnace and spent residue going to drains. Please confirm current Indonesian chemical-control and waste requirements with your regulatory adviser. Read the full SDS before handling.

09 / STORAGE & SHELF LIFE

Storing Logas dry, sealed and off the floor in Indonesia

General storage guidance for the rings. Your own EHS procedures and the batch SDS set the site-specific rules and re-test intervals.

Storage ConditionCool, dry, ventilated store; on pallets, off the floor
ContainerOriginal moisture-barrier packs, tightly closed
Typical Shelf Life12 months sealed, indicative
Keep Away FromWater, steam, acids
Beyond Retest DateRe-test moisture and ring strength

Moisture is the main enemy of a degassing ring. In humid Indonesian conditions an opened pack can take up water within days, rings may crumble and release gas unevenly, and wet rings can spit when plunged. Keep packs sealed until use, reseal part-used packs at once, store on pallets away from walls and roofs, and use stock first in, first out. Send any damp or crumbled stock for re-test or disposal rather than using it.

10 / PACKING & SHIPPING

Logas packing: moisture-barrier packs and cartons

Standard packing and shipping terms for the rings. Exact figures depend on origin, destination port and quantity and are confirmed with your order.

Standard PackingSealed packs in cartonsmoisture-barrier liner, typically 10 – 20 kg net
Small Packs1 kg and 5 kgfor trials and laboratories
PalletsWrapped and strappedprotected against moisture
Min. OrderFrom 500 kgtrial packs and samples on request
Lead Time2 – 4 weeksfrom order confirmation, plus transit
Shipment TypeTypical LoadBest ForNotes
Courier / air (samples)1 – 25 kgTrials, labsRegulatory class follows the batch SDS.
LCL (part container)1 – 8 tonnesFoundries and trial lotsPalletised and stretch-wrapped against moisture.
20′ FCL, 25 kg bagsAbout 18 – 22 tonnesLarge foundries and distributorsContainer liner or desiccant used on request.
Call-off contractsMonthly or quarterly lotsBuyers needing one consistent gradeAgreed specification and schedule; one manufacturing partner where possible.
11 / SUPPLY ACROSS INDONESIA

Logas supplier in Indonesia

Pengiriman ke seluruh Indonesia — delivery throughout Indonesia. We ship Logas to brass, bronze and copper-alloy foundries through the nearest major port, with onward trucking or inter-island shipping to your site.

Indonesian demand for copper-alloy degassing products comes from brass, bronze and valve foundries in Greater Jakarta, Tangerang, Cikarang, Karawang, Surabaya–Sidoarjo and Central Java, together with smaller casting shops across Sumatra, Kalimantan and Sulawesi.

Shipments land at Tanjung Priok, Tanjung Perak, Tanjung Emas or Batu Ampar for most buyers, or at Belawan and other regional ports, in closed, dry containers with palletised loads. Our desk shares quotations, CoA summaries and delivery updates in Bahasa Indonesia on request. See also Deoxidising Tubes and Slax 30 for the rest of the copper-alloy melt-treatment sequence.

RegionKey Cities & Industrial EstatesPort of DeliveryTypical Buyers
DKI JakartaJakarta, Pulogadung (JIEP), Marunda, CakungTanjung PriokFoundry consumable traders, brass casters
BantenCilegon (KIEC), Serang, Cikande, Tangerang, BalarajaMerak / Ciwandan · Tanjung PriokBrass and bronze foundries, valve makers
West JavaBekasi, Cikarang (Jababeka, MM2100, EJIP, Delta Silicon), Karawang (KIIC, Suryacipta), Purwakarta, BandungTanjung Priok · PatimbanValve, pump and fitting casters
Central JavaSemarang (Wijayakusuma), Kendal Industrial Park, Batang, SoloTanjung EmasFoundries and hardware casters
East JavaSurabaya (SIER), Gresik (JIIPE), Sidoarjo, Pasuruan (PIER), Mojokerto (Ngoro)Tanjung PerakBrass, bronze and pump casters
Riau IslandsBatam (Batamindo, Kabil), BintanBatu Ampar (Batam)Metal-casting users
North SumatraMedan (KIM), Kuala Tanjung, Sei MangkeiBelawan · Kuala TanjungFoundry distributors
Riau & South SumatraDumai, Pekanbaru, PalembangDumai · Boom Baru (Palembang)Foundry distributors
LampungBandar Lampung, Tanjung BintangPanjangRegional foundry distributors
KalimantanBalikpapan (Kariangau), Bontang, Samarinda, Banjarmasin, PontianakSemayang · Trisakti · PontianakRegional foundries
SulawesiMakassar (KIMA), Bitung, MorowaliMakassar New Port · BitungRegional casting shops and distributors
Import 01

HS Code & Customs

Degassing rings are typically classified under heading 3810 (fluxes and auxiliary preparations for metal treatment) or 3824, depending on composition. Your PPJK broker confirms the national subheading; invoice, packing list, CoA and SDS are drawn up to match, and an ATIGA Form D is issued where origin qualifies.

Import 02

Transport Class & SDS

The transport class follows Section 14 of the batch SDS and depends on the blend and grade. Where the lot is regulated we provide the declaration, labels and placards; where it is not, we say so in writing.

Import 03

Industrial Supply & Regulated End Uses

We supply Logas as a foundry consumable and ask about end use and site permits before quoting. Chemical-control, air-emission and waste rules apply at your site; please confirm current requirements with your regulatory adviser.

Import 04

Delivery to Foundry Centres

Java plants are served through Tanjung Priok, Tanjung Emas or Tanjung Perak; Batam direct through Batu Ampar; Sumatra and Kalimantan users direct or by transhipment, in dry, closed containers.

Delivery Cities in Indonesia

JakartaTangerangCilegonSerangBekasiCikarangKarawangPurwakartaBandungSemarangKendalSoloSurabayaGresikSidoarjoPasuruanMojokertoBatamBintanMedanDumaiPekanbaruPalembangBandar LampungBalikpapanBontangSamarindaBanjarmasinPontianakMakassarBitung
12 / QUALITY & DOCUMENTATION

What travels with every batch

The specification is agreed before the purchase order, not discovered on arrival. Every shipment of Logas leaves with a documented, checkable paper trail.

Doc 01

Certificate of Analysis

Batch-wise ring weight, dimensions, moisture, breakage and composition class, with manufacturing date, issued against the agreed specification so your QC team can check it rather than just file it.

Doc 02

Safety Data Sheet

GHS-format SDS in English covering hazard classification, handling, storage, first aid and spill response for the exact ring formulation shipped.

Doc 03

Technical Data Sheet

Reference properties, specification, storage and handling guidance, and typical use notes your technical or regulatory team can request.

Doc 04

Certificate of Origin

States the country of manufacture for customs clearance and any preferential-duty claim at your Indonesian port of discharge.

Doc 05

Transport Documents

Where the batch is classified, the declaration, labels and container packing certificate are prepared before loading; where it is not, we confirm that in writing.

Doc 06

Third-Party Inspection

Independent pre-shipment inspection and re-sampling can be arranged on request, at your cost, for buyers whose policy requires it.

13 / HOW ORDERING WORKS

From enquiry to delivery

A typical first order for Logas, whether it is going to Jakarta, Cikarang, Karawang, Surabaya or Batam.

Enquiry

Send grade, specification, quantity, packing, destination port or plant and your end use. The end use tells us which properties matter and whether any site or regulatory restriction needs to be considered.

Quotation

Most enquiries are quoted within one working day, with specification, price basis, Incoterm, lead time and payment terms in writing.

Sample & Specification Sign-off

Pre-shipment samples and a typical CoA can be sent so your QC team can test the grade in your own process and approve it before you commit to volume.

Purchase Order & Booking

Once the PO is confirmed we book container space, prepare labels and paperwork, and share the vessel schedule.

Dispatch & Documents

Bill of lading, commercial invoice, packing list, CoA, SDS, transport declaration where applicable and certificate of origin are sent ahead of arrival.

Delivery & After-Sales

We track the shipment to your port or plant and handle any documentation or quality queries after arrival.

14 / FAQ

Logas FAQs: copper degassing rings, storage, safety and price

What industrial buyers in Indonesia most often ask our sales desk about Logas.

01What is Logas and what is it used for?+
Logas is a pressed degassing ring for copper and copper-alloy melts. Plunged below the surface, it releases gas that carries dissolved hydrogen out of the metal and helps float oxides, reducing porosity in castings. We supply it to foundries across Indonesia.
02Can Logas be used for aluminium?+
No. It is made for copper alloys. For aluminium melts we supply Degasar, a degassing tablet made for that chemistry.
03How is Logas different from Deoxidising Tubes?+
Logas removes dissolved hydrogen. Deoxidising Tubes remove dissolved oxygen. Many copper-alloy foundries use both, along with a slag coagulant.
04Which copper alloys can be treated?+
Brass, bronze, gunmetal and copper are typical. Some alloys, such as aluminium bronzes, may need a different treatment, so tell us the alloy and we confirm suitability before quoting.
05How is the ring used?+
It is held on a plunger rod and pushed to the bottom of the melt until the reaction finishes. Practice varies, so we give no process doses; follow your technical team or the manufacturer’s guidance.
06What ring sizes are available?+
Weights and diameters are agreed per order to match your plunger and crucible, with tolerances shown on the CoA.
07Why must the rings be dry?+
Damp rings and wet plungers can spit or cause violent steam release in molten metal, and damp rings crumble. Dryness is the first value to read on the CoA.
08How should Logas be stored in Indonesia?+
Keep rings in sealed moisture-barrier packs in a cool, dry store on pallets, away from water and acids. Reseal part-used packs at once and use stock first in, first out.
09What safety precautions apply?+
Use dry, preheated tools, a face shield, heat-resistant gloves and an apron, and extract fume above the furnace. The SDS for your batch gives the classification for the formulation supplied.
10Does slag need separate treatment?+
Yes. After degassing, slag is coagulated with a product such as Slax 30 so it can be skimmed cleanly.
11What quality tests matter most for Logas?+
Ring weight, dimensions, moisture, breakage, strength and gas release, with the composition class from the SDS. Every shipment carries a certificate of analysis.
12What is the price of Logas in Indonesia?+
The price depends on formulation, ring size, packing, quantity, origin and delivery point at the time of order. Send us your requirement through the contact page and we will quote CFR, CIF or DAP in writing, usually within one working day.
13What packing, minimum order and lead time apply, and can I get a sample?+
Rings are packed in moisture-barrier packs in cartons. Orders start from about 500 kg, lead time is typically two to four weeks plus transit, and samples with a batch CoA are available.
14Are there regulatory restrictions on degassing rings in Indonesia?+
Rules depend on the formulation and on your site’s emissions and waste permits. We supply Logas as a foundry consumable, ask about the end use before quoting, and ask you to confirm current requirements with your regulatory adviser.
Request This Grade · Minta Penawaran

Buy Logas degassing rings in Indonesia: dry, consistent, on spec and on time

Send us your required grade, quantity, packing preference, end use and port or plant location anywhere in Indonesia. Our desk quotes most enquiries within one working day.